Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 11.51 MPa | 1669 psi | DCBP Cure |
Shin-Etsu Silicones KE-561U Silicone Elastomer KE561U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill.. |
|||
Tensile Strength at Break | 11.51 MPa | 1669 psi | DBPH Cure |