Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.00 - 11.0 MPa | 1020 - 1600 psi | ASTM D412 |
Proto3000 Objet Digital Materials™ DM_9130/9430/9230/9330 Rubber-like Prototyping Polymer Primary material: TangoBlackSecondary material: VeroWhitePlus, VeroBlue, VeroBlack, FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific concen.. |
|||
Tensile Strength at Break | 9.00 - 11.0 MPa | 1310 - 1600 psi | ISO 527-1 |
Adamas Adalon® 453 PTFE, Mica filler Information provided by Adamas, HPM |