Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.387 MPa | 1506.5 psi | Air at 257°F, 168 hr; ASTM D573 |
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |