Tensile Strength at Break 1440 MPa
209000 psi
Goodfellow Tungsten Carbide/Cobalt
Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard cerami..