Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.51 MPa | 2105 psi | |
Taiwan PU Corporation CPU-69-A/B Mixing Ratio 100/36 Polyurethane Casting Elastomer Compound of CPU-69-A/B with a mixing ratio of 100/36.Information provided by Taiwan PU Corporation.MatWeb has a separate entry for the unmixed A nd B components. |