Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.41 MPa | 2090 psi | Post Cure 16 Hours @ 232°C |
3M Dyneon™ RA 5300 High Performance Rubber Additive 3M™ Dynamar™ RA 5300 High Performance Rubber Additive is designed for use at low loadings to improve the processing in extrusion and molding operations. It utilizes unique chemistry which makes it.. |