Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.163 MPa | 1329 psi | |
Shin-Etsu Silicones SV-15000U Silicone Rubber SV15000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat.. |