Polymer Property : Tensile Strength at Break = 13.13 MPa
Polymer Property :
Tensile Strength at Break =
13.13 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
13.13
MPa
1904
psi
ISO R 527
Stir SpA SA 68 R CZ (PVC)
Application: Extrusion ecological sheath CEI 20-11 type TM 2Information provided by STIR SpA