Polymer Property : Tensile Strength at Break = 13.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.00 - 13.0 MPa
1310 - 1890 psi
ASTM D412
Proto3000 Objet Digital Materials™ DM_9610 Rubber-like Prototyping Polymer
Primary material: TangoGraySecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the..