Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 129.6 MPa | 18800 psi | ASTM D638 |
Covestro Petlon® DP3-1042 Semi-Crystalline PET, 40% Mineral/Glass Fiber
(discontinued **) Characteristics: General Purpose: Good Strength and Dimensional Stability, Low WarpageApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperatur.. |