Tensile Strength at Break 8.867 MPa

@Temperature 100 °C,
Time 605000 sec
1286 psi

@Temperature 212 °F,
Time 168 hour
After Dry Heat Aging; ASTM D865
Seals Eastern 7284 Butyl and Halobutyl Rubber
Chlorobutyl; High damping; Non-conductiveInformation provided by Seals Eastern, Inc.