Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 12.47 MPa @Temperature 100 °C, Time 605000 sec |
1808 psi @Temperature 212 °F, Time 168 hour |
After Dry Heat Aging; ASTM D865 |
Seals Eastern 7282 Neoprene / Chloroprene UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc. |