Mechanical Properties Metric English Comments
Tensile Strength at Break >= 794.3 MPa
>= 115200 psi
43.8 lb. Minimum Tensile Load 0.022 in. Diameter
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 30 lb
Best balance of toughness and strength. Low stretch for fast hook ups. High abrasion resistance. High knot efficiencyInformation provided by Shakespeare Company.