Mechanical Properties Metric English Comments
Tensile Strength at Break 113.75 MPa
16498 psi
ASTM D3756
3M 2497ST High-Temperature Tear Resistant Polyester Tape
3M™ High-Temperature Tear Resistant Polyester Tape 2497ST is designed for use in masking applications where sliver resistance and clean removal are required.Information provided by 3M