Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 76.5 MPa @Thickness 3.20 mm |
11100 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® SG5152 PBT+PET+GF15% Description: Injection Molding, PBT+PET+GF15%, Good Surface, High ImpactApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Tensile Strength at Break | 76.7 MPa | 11100 psi | ASTM D3759 |
3M 685 Riveters Tape 3M™ Riveters Tape 685 is a zone-coated polyester film tape with a tack-free center “window” for use in holding rivets in place both prior to and during riveting.Information provided by 3M |
|||
Tensile Strength at Break | 76.5 MPa | 11100 psi | ASTM D3759 |
3M 5181 General Purpose PTFE Skived Film Tapes 3M™ General Purpose PTFE Skived Film Tapes are film backing with a silicone adhesive.Information provided by 3M |