Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 107000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 738 MPa
107000 psi
2.1 lb. load and 0.005 in. diameter
Shakespeare WonderThread® SN-38 High tenacity TEX# 14 Nylon Industrial Sewing Thread
Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b..
Tensile Strength at Break 738 MPa
107000 psi
Shakespeare WP-200 diameter 0.2 mm Weft Polyester Monofilament
Paper Machine Clothing MonofilamentStandard molecular weightPolyesterModerate ModulusModerate shrinkage Information provided by Shakespeare Company.
Tensile Strength at Break 738 MPa
107000 psi
Shakespeare WP-320 diameter 0.2 mm Weft Polyester Monofilament
Paper Machine Clothing MonofilamentHigh molecular weightPolyesterWarp yarnHigh shrinkage Information provided by Shakespeare Company.