Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.343 MPa | 1065 psi | |
Shin-Etsu Silicones KE-941U Silicone Elastomer KE941 U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).Pr.. |
|||
Tensile Strength at Break | 7.343 MPa @Time 7200 sec |
1065 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 55-LR-9 TPE Product Description: StarTUFF TF 55-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |