Tensile Strength at Break 717 MPa
104000 psi
Annealed
Special Metals NILO® 365 Controlled-Expansion Alloy
For the manufacture of tooling for composites, the NILO® nickel-iron alloys offer a unique combination of matched thermal expansion to avoid warping during the curing cycle, along with strength, ..
Tensile Strength at Break 718 MPa

@Temperature 760 °C,
Time 3.60e+6 sec
104000 psi

@Temperature 1400 °F,
Time 1000 hour
Room Temperature properties after Isothermal Exposure
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar..