Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.10 MPa | 1030 psi | ASTM D412 |
Multibase TPSiV™ 3010-50A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tensile Strength at Break | 7.11 MPa | 1030 psi | ISO R 527 |
Stir SpA B 3015 AT S (PVC) Application: Molding for hairdresser/shower capsInformation provided by STIR SpA |
|||
Tensile Strength at Break | 7.08 MPa | 1030 psi | ISO R 527 |
Stir SpA PVGUM 26 ATC S (PVC) Application: TV shells with NitrileInformation provided by STIR SpA |
|||
Tensile Strength at Break | 7.10 MPa | 1030 psi | ASTM D412 |
Teknor Apex Monprene® MP-1358D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.10 MPa | 1030 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Tensile Strength at Break | 7.10 MPa | 1030 psi | ASTM D412 |
Teknor Apex Telcar® TL-2555F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 7.10 MPa | 1030 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Tensile Strength at Break | 7.10 MPa | 1030 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |