Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 702.6 MPa | >= 101900 psi | 8 lb. Minimum Tensile Load 0.01 in. Diameter |
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 6 lb Best balance of toughness and strength. Low stretch for fast hook ups. High abrasion resistance. High knot efficiencyInformation provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 702.6 MPa | >= 101900 psi | 18 lb. Minimum Tensile Load 0.015 in. Diameter |
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 15 lb 100% pure PVDF fluoro-polymer, great clarity, limpness and strength, low refractive index that decreases the visibility of the line.Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 702.6 MPa | >= 101900 psi | 50 lb. Minimum Tensile Load 0.025 in. Diameter |
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 40 lb Excellent castability and strength. Economic.Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 702.6 MPa | >= 101900 psi | 8 lb. Minimum Tensile Load 0.01 in. Diameter |
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 6 lb Excellent castability and strength. Economic.Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 702.6 MPa | >= 101900 psi | 32 lb. Minimum Tensile Load 0.02 in. Diameter |
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 25 lb Low stretch, high knot strength, shock strength, abrasion resistance, superior clarity.Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 702.6 MPa | >= 101900 psi | 8 lb. Minimum Tensile Load 0.01 in. Diameter |
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 6 lb Soft, limp and low line memory. Excellent cold casting properties. Especially designed for reels with tight arbors (example: micro spin casting reels)Information provided by Shakespeare Company. |