Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.8 MPa @Temperature 23.0 °C |
1570 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - .. |
|||
Tensile Strength at Break | 10.8 MPa | 1570 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3821 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 10.8 MPa | 1570 psi | ASTM D882-84 |
DuPont Elvax® 40L-08 Ethylene-Vinyl Acetate Copolymer Resin
(discontinued **) Elvax® 40L-08 is an ethylene-vinyl acetate copolymer that is useful in many wire and cable applications because of its excellent mechanical, thermal, and low-smoke properties. The melt index is ap.. |
|||
Tensile Strength at Break | 10.8 MPa | 1560 psi | |
Shin-Etsu Silicones KE-5006BU Low Temperature Silicone Elastomer ShinEtsu KE5006B U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Tensile Strength at Break | 10.8 MPa | 1560 psi | ASTM D412 |
Teknor Apex Monprene® MP-1848R Thermoplastic Elastomer Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to.. |
|||
Tensile Strength at Break | 10.8 MPa | 1560 psi | ASTM D412 |
Teknor Apex Telcar® TL-1425A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 10.8 MPa @Thickness 1.91 mm |
1560 psi @Thickness 0.0750 in |
20 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1934A Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Flexible Cord Jacketing; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581Forms: P.. |
|||
Tensile Strength at Break | 10.8 MPa | 1570 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Tensile Strength at Break | 10.8 MPa | 1560 psi | ASTM D3574 |
3M 3294 Vent Tape 3M™ Vent Tape 394 is a non-woven, synthetic backing with a strip-coated low-tack pressure sensitive adhesive for use in various venting applications requiring high outgassing rates.Information prov.. |
|||
Tensile Strength at Break | 10.8 MPa | 1570 psi | ASTM D638 |
3M Scotchkote™ FB 857 Urethane Floor Coating Scotchkote Urethane Floor Coating FB 857 has been specifically developed as a 100% solids protection system with a degree of flexibility for application to concrete and asphalt floor surfaces.Produc.. |