Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.07 MPa | 155 psi | Standard Cure; STM 40-107 |
3M AC-645 B-2 Aerospace Sealant 3M Aerospace Sealant AC-645 B-2 is a low density, two-component, manganese dioxide cured, liquid polysulfide polymer system. It is suitable for use in fuel tanks, fuselage hole filling, cavity filli.. |