Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.552 MPa | 80.0 psi | ASTM D412 |
Parker Chomerics CHO-FORM 5526 EMI Shielding Material Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Tensile Strength at Break | >= 0.552 MPa | >= 80.0 psi | ASTM D412 |
Parker Chomerics CHO-SEAL 1501 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |