Polymer Property : Tensile Strength at Break = 0.500 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.500 - 1.50 MPa
72.5 - 218 psi
ASTM D412
Proto3000 Objet Digital Materials™ DM_9840/9740 Rubber-like Prototyping Polymer
Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu..
Tensile Strength at Break 0.500 - 1.50 MPa
72.5 - 218 psi
ASTM D412
Proto3000 Objet Digital Materials™ DM_9850/9750 Rubber-like Prototyping Polymer
Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu..
Tensile Strength at Break 0.500 - 1.00 MPa
72.5 - 145 psi
ASTM-D828
GrafTech GRAFCELL® GDB Graphite Gas Diffusion Barrier
GRAFCELL® Gas Diffusion Barrier (GDB) material is a thin, perforated structure made from a continuous matrix of expanded natural graphite with excellent electrical conductivity, thermal conductiv..