Polymer Property : Tensile Strength at Break = 0.0276 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.0276 MPa
4.00 psi
Abatron AboSeal 8104-18 Vinyl-Acrylic-Latex Based Sealant and Caulk
AboSeal 8104-18 is 81% solids and vinyl-acrylic-latex based. It comes as one package, is available in most colors, and is lower cost. It has low odor and no sag, bonds to many surfaces without prime..