Polymer Property : Izod Impact, Unnotched = 9.81 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched >= 9.81 J/cm

@Temperature 23.0 °C
>= 18.4 ft-lb/in

@Temperature 73.4 °F
ISO 180
LG Chemical MB838A Opaque impact modifier
Description: MBS type opaque impact modifiers from LG Chem are appropriate for improving impact strength all the PVC products of rigid and semi-rigid opaque PVC, and have differentiated characterist..
Izod Impact, Unnotched 9.81 J/cm
18.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP)
LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers.