Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.10 J/cm

@Thickness 3.18 mm
9.55 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
Izod Impact, Unnotched 5.10 J/cm
9.55 ft-lb/in
ASTM D256
Chevron Phillips Xtel® XK2040 Polyphenylene Sulfide Alloy  (discontinued **)
Natural Color Polyphenylene Sulfide AlloyXtel™ XK2040 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties alo..
Izod Impact, Unnotched 5.10 - 5.10 J/cm

@Temperature -40.0 - -40.0 °C
9.55 - 9.55 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 5.10 J/cm Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..