Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.88 J/cm | 9.14 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DE0049F PC LNP* STAT-KON* DE0049F is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior, Molding... |
|||
Izod Impact, Unnotched | 4.88 J/cm | 9.14 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |