Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.96 J/cm | 16.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DX06410 PC (Asia Pacific) LNP* Thermocomp* DX06410 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched | 8.96 J/cm | 16.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DX06410 PC LNP* THERMOCOMP* DX06410 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |