Mechanical Properties Metric English Comments
Izod Impact, Unnotched 8.90 J/cm

@Temperature 23.0 °C
16.7 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Valox® 175 PBT
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 8.90 J/cm
16.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East)
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.
Izod Impact, Unnotched 8.90 J/cm
16.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 176 PBT
Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Izod Impact, Unnotched 8.90 J/cm
16.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 176HP PBT
Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Izod Impact, Unnotched 8.90 J/cm
16.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON FD000 PE
LNP* STAT-KON* FD000 is an unfilled Polyethylene. Added feature of this grade is: Electrically Conductive.