Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.84 J/cm | 16.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 LNP* THERMOCOMP* RC004SXS is a compound based on Nylon 66 containing 20% Carbon Fiber. Added feature of this grade includes: Heat Stabilized, Electrically Conductive. |