Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.68 J/cm
8.77 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DEP32 PC
LNP* STAT-KON* DEP32 is a compound based on Polycarbonate containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.