Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.67 J/cm @Temperature 23.0 °C |
16.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6 (Asia Pacific) LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Izod Impact, Unnotched | 8.67 J/cm | 16.2 ft-lb/in | ASTM D4812 |