Polymer Property : Izod Impact, Unnotched = 8.63 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 8.63 J/cm
16.2 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP LC008EXQ PEEK
LNP* THERMOCOMP* LC008EXQ is a compound based on Polyetheretherketone containing 40% Carbon Fiber. Added features of this grade include: Electrically Conductive, Easy Molding.