Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.48 J/cm | 8.40 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.48 J/cm | 8.40 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.48 J/cm | 8.40 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.48 J/cm | 8.40 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.48 J/cm | 8.40 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.48 J/cm | 8.40 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |