Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.23 J/cm | 15.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF004 is a compound based on Nylon 6/12 resin containing Glass Fiber. |