Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.588 - 8.17 J/cm
1.10 - 15.3 ft-lb/in
Average value: 5.62 J/cm Grade Count:16
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..