Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.07 J/cm | 15.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear.. |
|||
Izod Impact, Unnotched | 8.07 J/cm | 15.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP PFW64 PA 6 LNP* THERMOCOMP* PFW64 is a compound based on Nylon 6 resin containing 20% Glass Fiber, 30% Wollastonite. |