Polymer Property : Izod Impact, Unnotched = 7.64 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.08 J/cm

@Temperature 23.0 °C
7.64 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp EFP36G PEI
LNP* EFP36G is a Polyetherimide base resin containing a Mixed Glass Fiber and PTFE/Silicone.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 4.08 J/cm

@Temperature 23.0 °C
7.64 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Stat-kon DEL369E PC
LNP* Stat-Kon* DEL369E is a compound based on Polycarbonate containing Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant and Statically Conductive.This data was supplied by S..
Izod Impact, Unnotched 4.08 J/cm

@Temperature 23.0 °C
7.64 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific)
LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched 4.08 J/cm

@Temperature 23.0 °C
7.64 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6
LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 4.08 J/cm

@Temperature 23.0 °C
7.64 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6 (Asia Pacific)
LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.