Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.55 J/cm | 14.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF0069P PC LNP THERMOCOMP* DF0069P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |