Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.94 J/cm | 7.38 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP LNP* THERMOCOMP* MX88028 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Izod Impact, Unnotched | 3.94 J/cm | 7.38 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP (Asia Pacific) LNP* Thermocomp* MX88028 is a compound based on Polypropylene resin containing Glass Fiber. |