Polymer Property : Izod Impact, Unnotched = 7.27 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 7.27 J/cm
13.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6
LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact.