Polymer Property : Izod Impact, Unnotched = 7.22 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 7.22 J/cm
13.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DF008 PC
LNP THERMOCOMP* DF008 is a compound based on Polycarbonate resin containing 40% Glass Fiber.