Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Izod Impact, Unnotched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Unnotched | 7.15 J/cm @Temperature 23.0 °C |
13.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66 LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |