Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.92 J/cm @Temperature 23.0 °C |
13.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |