Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.70 J/cm @Thickness 3.17 mm |
12.6 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Performance Polymers IPS II PPL-C4219 PEKK (Polyetherketoneketone) Linear Wear Grade Black pellets; Carbon fiber/PTFE/Graphite compoundInformation provided by Infinite Polymer System II. |