Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.40 - 3.40 J/cm @Temperature -30.0 - -30.0 °C |
6.37 - 6.37 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 3.40 J/cm Grade Count:1 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |