Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.28 J/cm | 6.14 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA LNP THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
Izod Impact, Unnotched | 3.28 J/cm | 6.14 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA (Asia Pacific) LNP* THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |