Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.01 J/cm
5.64 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66
LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive.