Polymer Property : Izod Impact, Unnotched = 5.58 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.58 J/cm
10.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET
LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant.